ISO 806:2004Published

Aluminium oxide primarily used for the production of aluminium — Determination of loss of mass at 300 degrees C and 1 000 degrees C

Oxyde d'aluminium principalement utilisé pour la production de l'aluminium — Détermination de la perte de masse à 300 degrés C et à 1 000 degrés C

Abstract / scope

ISO 806:2004 specifies a method for the determination of loss of mass on heating of aluminium oxide at 300 °C and further loss of mass on ignition at 1 000 °C. By industry convention, these mass losses are often referred to as "moisture (MOI)" and "loss on ignition (LOI)" respectively.

This method is suitable for calcined alumina in the range 0,2 % to 5 % loss of mass at 300 °C and 0,1 % to 2 % loss of mass at 1 000 °C.

This method provides for samples to be treated on an "as-received" basis for determination of actual MOI and LOI in alumina samples. To improve precision of analysis in cases where "as-received" results are not required, samples can be "air-equilibrated" prior to analysis. "Air-equilibration" can greatly affect MOI results and significantly alter LOI results. The "air-equilibration" procedure and its effects are discussed.

Instrumental methods are also discussed.

Life cycle

Replaces

ISO 803:1976WithdrawnAluminium oxide primarily used for the production of aluminium — Determination of loss of mass at 300 degrees C (conventional moisture)International Standard · Published 1 Sep 1976 · ISO/TC 226ISO 806:1976WithdrawnAluminium oxide primarily used for the production of aluminium — Determination of loss of mass at 1 000 degrees C and 1 200 degrees CInternational Standard · Published 1 Sep 1976 · ISO/TC 226