Abstract / scope
A test portion of resin is spreaded out in a weighing dish, weighed to the nearest 0,000 5 g and dried at 110 °C to constant mass. The volatile matter is expressed as percentage of the original weight.
Plastiques — Résines d'homopolymères et de copolymères de chlorure de vinyle — Détermination des matières volatiles (y compris l'eau)
A test portion of resin is spreaded out in a weighing dish, weighed to the nearest 0,000 5 g and dried at 110 °C to constant mass. The volatile matter is expressed as percentage of the original weight.