ISO 5618-2:2024Published

Fine ceramics (advanced ceramics, advanced technical ceramics) — Test method for GaN crystal surface defects — Part 2: Method for determining etch pit density

Céramiques techniques — Méthode d’essai pour les défauts de surface des cristaux de GaN — Partie 2: Méthode de détermination de la densité des piqûres

Abstract / scope

This document describes a method for determining the etch pit density, which is used to detect dislocations and processing-introduced defects that occur on single-crystal GaN substrates or single-crystal GaN films.

It is applicable to the defects specified in ISO 5618-1 from among the defects exposed on the surface of the following types of GaN substrates or films: single-crystal GaN substrate; single-crystal GaN film formed by homoepitaxial growth on a single-crystal GaN substrate; or single-crystal GaN film formed by heteroepitaxial growth on a single-crystal Al2O3, SiC, or Si substrate.

It is applicable to defects with an etch pit density of ≤ 7 × 107 cm-2.